Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
Ti-13V-11Cr-3Al
Category Titanium Alloy
Class Wrought
Type Beta alloy
Designations United States: MIL-T-9046, AMS 4917

Composition
ElementWeight %
V  13 
Cr  11 
Al  3 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 4.84 25  
Poisson's Ratio 0.3 25  
Elastic Modulus (GPa) 101.4 25  
Tensile Strength (Mpa) 1276  25  solution+age  
Yield Strength (Mpa) 1207 
Elongation (%)
Reduction in Area (%)  
Hardness (HRC) 40  25  solution+age 
Impact Strength (J)
(Charpy)
11  25  solution+age  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 9.4  20-100 more  
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.