Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Further Details
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
Ti-3Al-8V-6Cr-4Mo-4Zr
Conditions Tensile Properties 
T (°C)Treatment
25 annealed   Tensile Strength (MPa) 883 
Yield Strength (MPa) 834 
Elongation (%) 15 
Reduction in Area (%)  
25 solution+ age   Tensile Strength (MPa) 1448 
Yield Strength (MPa) 1379 
Elongation (%)
Reduction in Area (%)  
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!