Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
Ti-0.3Mo-0.8Ni
Category Titanium Alloy
Class Wrought
Type Commercially Pure

Composition
ElementWeight %
Mo  0.3 
Ni  0.8 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 4.54 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 100-120 25  
Tensile Strength (Mpa) 324  315 more annealed  
Yield Strength (Mpa) 207 
Elongation (%) 32 
Reduction in Area (%)  
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.