Metal Alloys
Alloy Home
Steels
Tool Steels
General Information
Properties
Tool Steel Types
High-Speed
Hot-Work
Cold-Work
Shock-Resistant
Mold
Special-Purpose
Water-Hardening
Tool Steel List
AISI Ax
AISI Dx
AISI Hx
AISI Lx
AISI Mx
AISI Ox
AISI Px
AISI Sx
AISI Tx
AISI Wx
Specific Tool Steel
General Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AISI H13
Category Steel
Class Tool steel
Type Chromium hot work steel
Designations  France: AFNOR Z 40 COV 5
Germany: DIN 1.2344
Italy: UNI KU
Japan: JIS SKD61
Sweden: SS 2242
United Kingdom: B.S. BH 13
United States: ASTM A681 , FED QQ-T-570 , SAE J437 , SAE J438 , SAE J467 , UNS T20813

Composition
ElementWeight %
C  0.32-0.45 
Mn  0.20-0.50 
Si  0.80-1.20 
Cr  4.75-5.50 
Ni  0.3 
Mo  1.10-1.75 
V  0.80-1.20 
Cu  0.25 
P  0.03 
S  0.03 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.76 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 10.4  20-100 more  
Thermal Conductivity (W/m-K) 28.6  215 more  
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.