Metal Alloys
Alloy Home
Steels
Tool Steels
General Information
Properties
Tool Steel Types
High-Speed
Hot-Work
Cold-Work
Shock-Resistant
Mold
Special-Purpose
Water-Hardening
Tool Steel List
AISI Ax
AISI Dx
AISI Hx
AISI Lx
AISI Mx
AISI Ox
AISI Px
AISI Sx
AISI Tx
AISI Wx
Specific Tool Steel
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
AISI H22
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
20-100   11 
20-425   11.5 
20-540   12 
20-650   12.4 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.