Metal Alloys
Alloy Home
Steels
Tool Steels
General Information
Properties
Tool Steel Types
High-Speed
Hot-Work
Cold-Work
Shock-Resistant
Mold
Special-Purpose
Water-Hardening
Tool Steel List
AISI Ax
AISI Dx
AISI Hx
AISI Lx
AISI Mx
AISI Ox
AISI Px
AISI Sx
AISI Tx
AISI Wx
Specific Tool Steel
General Information
Further Details
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
AISI S2
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
20-100   10.9 
20-200   11.9 
20-425   13.5 
20-540   14 
20-650   14.2 
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.