| AISI S5 | |
![]() | |
| Conditions | Impact Energy (J) | ||
| T (°C) | Treatment | Method | Value |
| 25 | oil quenched from 870°C, single tempered at 205°C | Charpy unnotched | 206 |
| 25 | oil quenched from 870°C, single tempered at 315°C | Charpy unnotched | 232 |
| 25 | oil quenched from 870°C, single tempered at 425°C | Charpy unnotched | 243 |
| 25 | oil quenched from 870°C, single tempered at 540°C | Charpy unnotched | 188 |