Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
Introduction

Properties of common liquid materials are divided into following categories:

 

  • Physical properties: Density, melting and boiling temperature.
• Mechanical Properties: Poisson's Ratio, bulk modulus, viscousity, kinematic viscousity.
• Thermal Properties: Coefficient of thermal expansion, thermal conductivity.
• Electric Properties: Electric resistivity.
• Acoustic Properties: Sound velocity.
 

  Note: 1. All properties are under 1 atm (1.01325×105 Pa; 760 mmHg; 14.6959 psi) and at room temperature 25 ºC (77 ºF) unless specified otherwise.
  2. Further information on a specific material can be obtained by clicking the name of that particular material in the following table.
  3. Users who prefer Standard or other unit systems rather than the SI units, click the amount (number) of the specific material property for unit conversion.
  4. Materials in different phases at room temperature: Solid, Gas.
Basic Mechanical Properties
Material Bulk Modulus
(GPa)
Viscosity
(Pa-s)
Kinematic Viscosity
(m2/s)
Acetone [C3H6O] (20 ºC) - 0.389 × 10-3 -
Alcohol; Ethanol [C2H5OH] (20 ºC) 0.823 1.77 × 10-3 2.20 × 10-6
Alcohol; Methanol [CH3OH] (20 ºC) 0.902 0.817 × 10-3 1.01 × 10-6
Mercury [Hg] (20 ºC) 25.3 1.55 × 10-3 0.114 × 10-6
Oil; Lubricating (20 ºC) - 799 × 10-3 900 × 10-6
Water; Distilled [H2O] (20 ºC) 2.18 1.00 × 10-3 1.00 × 10-6
Water; Distilled [H2O] (4 ºC) - 1.57 × 10-3 1.57 × 10-6
Water; Sea (13 ºC) 2.28 - -
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.