Materials Home
Common Materials
Solids
Liquids
Gases
  Carbon Dioxide
Specific Materials
Elements
Metal Alloys
Polymers
Piezo Materials
Solders
Steam Tables
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 

Temp.
(ºC)
Density
(Kg/m3)
Viscosity
(Pa-s)
Kinematic Viscosity
(m2/s)
Gas Constant
(J/kg·K)
Constant Pressure Spectfic Heat
(J/kg·K)
Constant Volume Specific Heat
(J/kg·K)
Specific Heat Ratio
0 - 1.38 × 10-5 - 189 815 626 1.30
0 - 1.38 × 10-5 - 189 815 626 1.30
100 - 1.85 × 10-5 - 189 914 725 1.26
100 - 1.85 × 10-5 - 189 914 725 1.26
200 - 2.68 × 10-5 - 189 993 804 1.23
200 - 2.68 × 10-5 - 189 993 804 1.23
300 - - - 189 1060 868 1.22
300 - - - 189 1060 868 1.22
400 - - - 189 1110 921 1.21
400 - - - 189 1110 921 1.21
600 - - - 189 1190 1000 1.19
600 - - - 189 1190 1000 1.19
 
Note: 1. All properties are under 1 atm (1.01325×105 Pa; 760 mmHg; 14.6959 psi) unless specified otherwise.
  2. Users who prefer Standard or other unit systems rather than SI units, please click the amount (number) of the specific material property for unit conversion.
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.