Materials Home
Common Materials
Solids
Liquids
  Distilled Water
Gases
Specific Materials
Elements
Metal Alloys
Polymers
Piezo Materials
Solders
Steam Tables
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 

Temp.
(ºC)
Density
(×1000 Kg/m3)
Viscosity
(Pa-s)
Kinematic Viscosity
(m2/s)
Surface Tension
(N/m)
Bulk Modulus
(GPa)
Thermal Expansion Coefficient
(/ºC)
0 1 1.79 × 10-3 1.79 × 10-6 7.56 × 10-2 1.99 -6.81 × 10-5
0 1 1.79 × 10-3 1.79 × 10-6 7.56 × 10-2 1.99 -6.81 × 10-5
4 1 1.57 × 10-3 1.57 × 10-6 - - -
4 1 1.57 × 10-3 1.57 × 10-6 - - -
10 1 1.31 × 10-3 1.31 × 10-6 7.42 × 10-2 2.12 8.80 × 10-5
10 1 1.31 × 10-3 1.31 × 10-6 7.42 × 10-2 2.12 8.80 × 10-5
20 0.998 1.00 × 10-3 1.00 × 10-6 7.28 × 10-2 2.21 2.07 × 10-4
20 0.998 1.00 × 10-3 1.00 × 10-6 7.28 × 10-2 2.21 2.07 × 10-4
30 0.996 7.98 × 10-4 8.01 × 10-7 7.12 × 10-2 2.26 2.94 × 10-4
30 0.996 7.98 × 10-4 8.01 × 10-7 7.12 × 10-2 2.26 2.94 × 10-4
40 0.992 6.53 × 10-4 6.58 × 10-7 6.96 × 10-2 2.29 3.85 × 10-4
40 0.992 6.53 × 10-4 6.58 × 10-7 6.96 × 10-2 2.29 3.85 × 10-4
50 0.988 5.47 × 10-4 5.48 × 10-7 6.79 × 10-2 2.29 4.58 × 10-4
50 0.988 5.47 × 10-4 5.48 × 10-7 6.79 × 10-2 2.29 4.58 × 10-4
60 0.983 4.67 × 10-4 4.75 × 10-7 6.62 × 10-2 2.28 5.23 × 10-4
60 0.983 4.67 × 10-4 4.75 × 10-7 6.62 × 10-2 2.28 5.23 × 10-4
70 0.978 4.04 × 10-4 4.13 × 10-7 6.64 × 10-2 2.24 5.84 × 10-4
70 0.978 4.04 × 10-4 4.13 × 10-7 6.64 × 10-2 2.24 5.84 × 10-4
80 0.972 3.55 × 10-4 3.65 × 10-7 6.26 × 10-2 2.20 6.41 × 10-4
80 0.972 3.55 × 10-4 3.65 × 10-7 6.26 × 10-2 2.20 6.41 × 10-4
90 0.965 3.15 × 10-4 3.26 × 10-7 - 2.14 6.96 × 10-4
90 0.965 3.15 × 10-4 3.26 × 10-7 - 2.14 6.96 × 10-4
100 0.958 2.82 × 10-4 2.94 × 10-7 5.89 × 10-2 2.07 7.50 × 10-4
100 0.958 2.82 × 10-4 2.94 × 10-7 5.89 × 10-2 2.07 7.50 × 10-4
 
Note: 1. All properties are under 1 atm (1.01325×105 Pa; 760 mmHg; 14.6959 psi) unless specified otherwise.
  2. Users who prefer Standard or other unit systems rather than SI units, please click the amount (number) of the specific material property for unit conversion.
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.