Compare Reactions
To compare 2 reactions head to head, click on reactions from the list below.
 Element / Other   Reaction 
Electrode Potential (V)
(assumptions)
 Gold       Au+ + e-  =  Au    1.692 
 Gold       Au3+ + 3 e-  =  Au    1.498 
 Chlorine       Cl2(g) + 2 e-  =  2 Cl-    1.35827 
 Oxygen, Hydrogen (acid)       O2 + 4 H+ + 4 e-  =  2 H2O     1.229 
 Platinum       Pt2+ + 2 e-  =  Pt    1.18 
 Palladium       Pd2+ + 2 e-  =  Pd    0.951 
 Silver       Ag+ + e-  =  Ag    0.7996 
 Oxygen, Hydrogen (acid)       O2 + 2 H+ + 2 e-  =  H2O2     0.695 
 Copper       Cu+ + e-  =  Cu    0.521 
 Oxygen, Water       O2 + 2 H2O + 4 e-  =  4 OH-    0.401 
 Copper       Cu2+ + 2 e-  =  Cu    0.3419 
 Hydrogen (acid)       2 H+ + 2 e-  =  H2    0 
 Iron       Fe3+ + 3 e-  =  Fe    -0.037 
 Lead       Pb2+ + 2 e-  =  Pb    -0.1262 
 Tin       Sn2+ + 2 e-  =  Sn    -0.1375 
 Oxygen, Water       O2 + 2 H2O + 2 e-  =  H2O2 + 2 OH-    -0.146 
 Nickel       Ni2+ + 2 e-  =  Ni    -0.257 
 Cobalt       Co2+ + 2 e-  =  Co    -0.28 
 Cadmium       Cd2+ + 2 e-  =  Cd    -0.403 
 Iron       Fe2+ + 2 e-  =  Fe    -0.447 
 Chromium       Cr3+ + 3 e-  =  Cr    -0.744 
 Zinc       Zn2+ + 2 e-  =  Zn    -0.7618 
 Water       2 H2O + 2 e-  =  H2 + 2 OH-    -0.8277 
 Chromium       Cr2+ + 2 e-  =  Cr    -0.913 
 Manganese       Mn2+ + 2 e-  =  Mn    -1.185 
 Titanium       Ti3+ + 3 e-  =  Ti    -1.37 
 Titanium       Ti2+ + 2 e-  =  Ti    -1.63 
 Aluminum       Al3+ + 3 e-  =  Al    -1.662 
 Magnesium       Mg2+ + 2 e-  =  Mg    -2.372 
 Magnesium       Mg+ + e-  =  Mg    -2.7 
 Sodium       Na+ + e-  =  Na    -2.71 
 Calcium       Ca2+ + 2 e-  =  Ca    -2.868 
 Potassium       K+ + e-  =  K    -2.931 
 Lithium       Li3+ + e-  =  Li    -3.0401 
 Calcium       Ca+ + e-  =  Ca    -3.8 
Records 1 - 35 (of 35 found)
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!