Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
Actinium
89
Ac
[227]
Atomic Number 89
Atomic Weight [227]
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-10-0-2-6-1-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 10000 kg/m3 Solid  298.15  0 

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1324.15 K   101325 
Boiling Temperature 3471.15 K   101325 
Fusion Enthalpy 63 J/g 0  101325 
Heat Capacity 120 J/kg-K 298.149993896 100000 
 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.