Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Americium
95
Am
[243]
Atomic Number 95
Atomic Weight [243]
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-10-7-2-6-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 11870 kg/m3 Solid  298.15 

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1449.15 K   101325 
Boiling Temperature 2284.15 K   101325 
 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.