Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
Barium
56
Ba
137.327
Atomic Number 56
Atomic Weight 137.327
Electron Config. 2-2-6-2-6-10-2-6-10-0-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 3620 kg/m3 Solid  298.15 
Thermal Expansion Coefficient 2.060 /K Solid  298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1000.15 K   101325 
Boiling Temperature 2170.15 K   101325 
Critical Temperature 4450 K    
Fusion Enthalpy 52 J/g 101325 
Vaporization Enthalpy 1019.46 J/g 101325 
Heat Capacity 204 J/kg-K 298.149993896 100000 
Thermal Conductivity 18.4 W/m-K 300 101325 
 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.