Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
Bismuth
83
Bi
208.98
Atomic Number 83
Atomic Weight 208.98
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-10-0-2-3
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 9790 kg/m3 Solid  298.15 
Modulus of Elasticity 34.474 GPa Solid  0   
Poisson Ratio 0.33 Solid     
Thermal Expansion Coefficient 1.340 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.068 W-m 273.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 544.55 K   101325 
Boiling Temperature 1837.15 K   101325 
Critical Temperature 4450 K    
Fusion Enthalpy 54.1 J/g 101325 
Vaporization Enthalpy 722.56 J/g 101325 
Heat Capacity 122 J/kg-K 298.149993896 100000 
Thermal Conductivity 7.87 W/m-K 300 101325 
 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.