Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
Cerium
58
Ce
140.115
Atomic Number 58
Atomic Weight 140.115
Electron Config. 2-2-6-2-6-10-2-6-10-1-2-6-1-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 8160 kg/m3 Solid  298.15 
Modulus of Elasticity 41.369 GPa Solid  313.15   
Poisson Ratio 0.24 Solid     
Thermal Expansion Coefficient 5.200 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 7.500 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1072.15 K   101325 
Boiling Temperature 3697.15 K   101325 
Critical Temperature 9750 K    
Fusion Enthalpy 39 J/g 101325 
Heat Capacity 192 J/kg-K 298.149993896 100000 
Thermal Conductivity 11.3 W/m-K 300 101325 
 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.