Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Copper
29
Cu
63.546
Atomic Number 29
Atomic Weight 63.546
Electron Config. 2-2-6-2-6-10-1
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 8960 kg/m3 Solid  298.15 
Modulus of Elasticity 110.316 GPa Solid  0   
Thermal Expansion Coefficient 1.650 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.673 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1357.77 K   101325 
Boiling Temperature 2835.15 K   101325 
Critical Temperature 8280 K    
Fusion Enthalpy 208.7 J/g 101325 
Heat Capacity 385 J/kg-K 298.149993896 more... 100000 
Thermal Conductivity 401 W/m-K 300 more... 101325 
 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.