Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
Erbium
68
Er
167.26
Atomic Number 68
Atomic Weight 167.26
Electron Config. 2-2-6-2-6-10-2-6-10-12-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 9070 kg/m3 Solid  298.15 
Modulus of Elasticity 110.316 GPa Solid  0   
Poisson Ratio 0.24 Solid     
Thermal Expansion Coefficient 1.220 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.070 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1802.15 K   101325 
Boiling Temperature 3135.15 K   101325 
Critical Temperature 7250 K    
Fusion Enthalpy 119 J/g 101325 
Heat Capacity 168 J/kg-K 298.149993896 100000 
Thermal Conductivity 14.5 W/m-K 300 101325 
 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.