Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
Europium
63
Eu
151.965
Atomic Number 63
Atomic Weight 151.965
Electron Config. 2-2-6-2-6-10-2-6-10-7-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 5240 kg/m3 Solid  298.15 
Poisson Ratio 0.15 Solid     
Thermal Expansion Coefficient 3.500 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 9.000 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1095.15 K   101325 
Boiling Temperature 1869.15 K   101325 
Critical Temperature 4350 K    
Fusion Enthalpy 60.6 J/g 101325 
Heat Capacity 182 J/kg-K 298.149993896 100000 
Thermal Conductivity 14 W/m-K 300 101325 
 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.