Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
Fluorine
9
F
18.9984
Atomic Number 9
Atomic Weight 18.9984
Electron Config. 2-2-5
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density (F2) 1.696 kg/m3 Gas  293.15  101325 

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature (F2) 53.53 K   101325 
Boiling Temperature (F2) 85.03 K   101325 
Critical Temperature (F2) 144.13 K    
Fusion Enthalpy (F2) 13.4 J/g 101325 
Vaporization Enthalpy (F2) 174.23 J/g 101325 
Heat Capacity (F2) 824 J/kg-K 298.149993896 100000 
 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.