Element Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
Hafnium
72
Hf
178.49
Atomic Number 72
Atomic Weight 178.49
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-2-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 13300 kg/m3 Solid  298.15 
Poisson Ratio 0.37 Solid     
Thermal Expansion Coefficient 5.900 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 3.510 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 2506.15 K   101325 
Boiling Temperature 4876.15 K   101325 
Critical Temperature 10400 K    
Fusion Enthalpy 152.4 J/g 101325 
Heat Capacity 144 J/kg-K 298.149993896 100000 
Thermal Conductivity 23 W/m-K 300 101325 
 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.