Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free publications
Indium
49
In
114.818
Atomic Number 49
Atomic Weight 114.818
Electron Config. 2-2-6-2-6-10-2-6-10-0-2-1
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 7310 kg/m3 Solid  298.15 
Modulus of Elasticity 13.79 GPa Solid  0   
Thermal Expansion Coefficient 3.210 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 8.370 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 429.75 K   101325 
Boiling Temperature 2345.15 K   101325 
Critical Temperature 6150 K    
Fusion Enthalpy 28.6 J/g 101325 
Heat Capacity 233 J/kg-K 298.149993896 100000 
Thermal Conductivity 81.6 W/m-K 300 101325 
 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?