Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
Lutetium
71
Lu
174.967
Atomic Number 71
Atomic Weight 174.967
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-1-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 9840 kg/m3 Solid  298.15 
Poisson Ratio 0.26 Solid     
Thermal Expansion Coefficient 9.900 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 7.900 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1936.15 K   101325 
Boiling Temperature 3666.15 K   101325 
Fusion Enthalpy 106.6 J/g 101325 
Heat Capacity 154 J/kg-K 298.149993896 100000 
Thermal Conductivity 16.4 W/m-K 300 101325 
 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.