Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
Osmium
76
Os
190.23
Atomic Number 76
Atomic Weight 190.23
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-6-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 22590 kg/m3 Solid  298.15 
Modulus of Elasticity 558.476 GPa Solid  0   
Poisson Ratio 0.25 Solid     
Thermal Expansion Coefficient 5.100 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 9.500 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 3306.15 K   101325 
Boiling Temperature 5285.15 K   101325 
Critical Temperature 12700 K    
Fusion Enthalpy 304.2 J/g 101325 
Heat Capacity 130 J/kg-K 298.149993896 100000 
Thermal Conductivity 87.6 W/m-K 300 101325 
 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.