Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
Palladium
46
Pd
106.42
Atomic Number 46
Atomic Weight 106.42
Electron Config. 2-2-6-2-6-10-2-6-10
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 12000 kg/m3 Solid  298.15 
Modulus of Elasticity 110.316 GPa Solid  0   
Poisson Ratio 0.39 Solid     
Thermal Expansion Coefficient 1.180 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.080 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1828.05 K   101325 
Boiling Temperature 3236.15 K   101325 
Critical Temperature 7700 K    
Fusion Enthalpy 157.3 J/g 101325 
Heat Capacity 244 J/kg-K 298.149993896 100000 
Thermal Conductivity 71.8 W/m-K 300 101325 
 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!