Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
Promethium
61
Pm
[145]
Atomic Number 61
Atomic Weight [145]
Electron Config. 2-2-6-2-6-10-2-6-10-5-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 7260 kg/m3 Solid  298.15  0 
Poisson Ratio 0.28 Solid     
Thermal Expansion Coefficient 1.100 /K Solid  298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1315.15 K   101325 
Boiling Temperature 3273.15 K   101325 
Thermal Conductivity 15 W/m-K 300 101325 
 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.