Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
Praseodymium
59
Pr
140.908
Atomic Number 59
Atomic Weight 140.908
Electron Config. 2-2-6-2-6-10-2-6-10-3-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 6770 kg/m3 Solid  298.15 
Modulus of Elasticity 68.948 GPa Solid  0   
Poisson Ratio 0.28 Solid     
Thermal Expansion Coefficient 6.700 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 6.800 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1204.15 K   101325 
Boiling Temperature 3783.15 K   101325 
Critical Temperature 8900 K    
Fusion Enthalpy 48.9 J/g 101325 
Heat Capacity 193 J/kg-K 298.149993896 100000 
Thermal Conductivity 12.5 W/m-K 300 101325 
 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.