Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
Plutonium
94
Pu
[244]
Atomic Number 94
Atomic Weight [244]
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-10-6-2-6-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 19700 kg/m3 Solid  298.15  0 
Modulus of Elasticity 96.527 GPa Solid  298.15   
Poisson Ratio 0.21 Solid     
Thermal Expansion Coefficient 4.670 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.414 W-m 380.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 913.15 K   101325 
Boiling Temperature 3501.15 K   101325 
Critical Temperature 10500 K    
Fusion Enthalpy 11.7 J/g 0  101325 
Heat Capacity 140 J/kg-K 298.149993896 0 
Thermal Conductivity 6.74 W/m-K 300 101325 
 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!