Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
Rhenium
75
Re
186.207
Atomic Number 75
Atomic Weight 186.207
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-5-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 20800 kg/m3 Solid  298.15 
Modulus of Elasticity 461.949 GPa Solid  293.15   
Poisson Ratio 0.3 Solid     
Thermal Expansion Coefficient 6.200 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.930 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 3459.15 K   101325 
Boiling Temperature 5869.15 K   101325 
Critical Temperature 18900 K    
Fusion Enthalpy 324.5 J/g 101325 
Heat Capacity 137 J/kg-K 298.149993896 100000 
Thermal Conductivity 47.9 W/m-K 300 101325 
 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.