Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
Sulfur
16
S
32.066
Atomic Number 16
Atomic Weight 32.066
Electron Config. 2-2-6-2-4
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 2070 kg/m3 Solid  0  0 
Thermal Expansion Coefficient 6.400 /K Solid  293.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 2.000 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 388.36 K   101325 
Boiling Temperature 717.75 K   101325 
Critical Temperature 1314.15 K    
Fusion Enthalpy 53.4 J/g 0  101325 
Vaporization Enthalpy 1403.36 J/g 0  101325 
 
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.