Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
Scandium
21
Sc
44.9559
Atomic Number 21
Atomic Weight 44.9559
Electron Config. 2-2-6-2-6-1-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 2990 kg/m3 Solid  298.15  0 
Poisson Ratio 0.28 Solid     
Thermal Expansion Coefficient 1.020 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 6.100 W-m 295.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1814.15 K   101325 
Boiling Temperature 3103.15 K   101325 
Critical Temperature 6410 K    
Fusion Enthalpy 314 J/g 0  101325 
Heat Capacity 568 J/kg-K 298.149993896 100000 
Thermal Conductivity 15.8 W/m-K 300 101325 
 
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.