Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
Samarium
62
Sm
150.36
Atomic Number 62
Atomic Weight 150.36
Electron Config. 2-2-6-2-6-10-2-6-10-6-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 7520 kg/m3 Solid  298.15  0 
Modulus of Elasticity 55.158 GPa Solid  0   
Poisson Ratio 0.27 Solid     
Thermal Expansion Coefficient 1.270 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 8.800 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1345.15 K   101325 
Boiling Temperature 2063.15 K   101325 
Critical Temperature 5050 K    
Fusion Enthalpy 57.3 J/g 0  101325 
Heat Capacity 197 J/kg-K 298.149993896 100000 
Thermal Conductivity 13.3 W/m-K 300 101325 
 
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.