Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
Tellurium
52
Te
127.6
Atomic Number 52
Atomic Weight 127.6
Electron Config. 2-2-6-2-6-10-2-6-10-0-2-4
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 6240 kg/m3 Solid  0 
Modulus of Elasticity 41.369 GPa Solid  0   
Thermal Expansion Coefficient 1.675 /K Solid  293.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 0.004360 W-m 296.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 722.66 K   101325 
Boiling Temperature 1261.15 K   101325 
Critical Temperature 2330 K    
Fusion Enthalpy 137.1 J/g 101325 
Vaporization Enthalpy 894.20 J/g 101325 
Heat Capacity 202 J/kg-K 298.149993896 100000 
 
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.