Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
Vanadium
23
V
50.9415
Atomic Number 23
Atomic Weight 50.9415
Electron Config. 2-2-6-2-6-3-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 6000 kg/m3 Solid  298.15  0 
Modulus of Elasticity 131 GPa Solid  0   
Poisson Ratio 0.37 Solid     
Thermal Expansion Coefficient 8.400 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 2.540 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 2183.15 K   101325 
Boiling Temperature 3680.15 K   101325 
Critical Temperature 11300 K    
Fusion Enthalpy 422 J/g 0  101325 
Heat Capacity 489 J/kg-K 298.149993896 more... 100000 
Thermal Conductivity 30.7 W/m-K 300 101325 
 
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.