Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Xenon
54
Xe
131.29
Atomic Number 54
Atomic Weight 131.29
Electron Config. 2-2-6-2-6-10-2-6-10-0-2-6
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 5.896 kg/m3 Gas  293.15  101325 
Density 2953 kg/m3 Liquid  165.1  101325 

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 161.4 K   101325 
Boiling Temperature 165.11 K   101325 
Critical Temperature 289.73 K    
Fusion Enthalpy 17.5 J/g 101325 
Vaporization Enthalpy 96.12 J/g 101325 
Heat Capacity 158 J/kg-K 298.149993896 100000 
 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.