Lead Zirconate Titanate (PZT-5A)
Crystal symmetry class Uniaxial
Density 7750 kg/m3
Constitutive data is presented in the Strain-Charge format.
Compliance
16.4 -5.74 -7.22 0 0 0
-5.74 16.4 -7.22 0 0 0
-7.22 -7.22 18.8 0 0 0
0 0 0 47.5 0 0
0 0 0 0 47.5 0
0 0 0 0 0 44.3
*10-12 
Piezoelectric Coupling
0 0 0 0 584 0
0 0 0 584 0 0
-171 -171 374 0 0 0
*10-12 
Relative Permittivity
1730 0 0
0 1730 0
0 0 1700
,  8.854 *10-12 
For a description of the ordering convention used to layout the constitutive matrices, see Subscript Ordering.
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.