kilogram per cubic meter






7869.99988556 kg/m3 =


Density | ||
Symbol | Unit Name | |
7.87 | g/cm3 | gram per cubic centimeter |
7.87×106 | g/m3 | gram per cubic meter |
7870 | g/l | gram per liter |
7.87 | kg/dm3 | kilogram per cubic decimeter |
7.87 | kg/l | kilogram per liter |
7860.93 | oz (av.)/ft3 | ounce (av.) per cubic foot |
4.54915 | oz (av.)/in3 | ounce (av.) per cubic inch |
491.308 | lbm/ft3 | pound mass per cubic foot |
0.284322 | lbm/in3 | pound mass per cubic inch |
1.32653×104 | lbm/yd3 | pound mass per cubic yard |
78.8764 | lbm/gal (UK) | pound mass per gallon (UK) |
65.6783 | lbm/gal (US, liq.) | pound mass per gallon (US, liq.) |
15.2703 | slug/ft3 | slug per cubic foot |
8.83699×10-3 | slug/in3 | slug per cubic inch |
412.299 | slug/yd3 | slug per cubic yard |
7.87 | specific gravity |