Units Currencies
Constants
Units Home
Unit Conversion
List Units
List Categories
Currencies
Convert Units
SI System
Base Units
Derived Units
Prefixes
Numbers
Constants
Base-N
Fractions
Time / Decimal
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
ksi-sqrt(inch)
Symbol:  ksi-sqrt(in) 
Category:  Fracture toughness 
SI Equivalent:  1.09884×106 Pa-sqrt(m)
Dimension ML-0.5T-2 
 
Notes
This unit is used in fracture mechanics to provide an index of the stress at the crack tip. This index is commonly called the stress intensity factor.
Convert     ksi-sqrt(in)  
1 ksi-sqrt(in) =
Fracture toughness
  Symbol Unit Name
1.09884  MPa-sqrt(m)  MPa-sqrt(meter) 
1.09884×106  Pa-sqrt(m)  Pa-sqrt(meter) 
1000  psi-sqrt(in)  psi-sqrt(inch) 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.